Получить цену
ЗЕЛЕНЫЕ ТЕХНОЛОГИИ

Высвобождение материала литиевой батареи во время дробления и разделения

Получить решение
Высвобождение материала литиевой батареи во время дробления и разделения
  • Емкость 500–1000 кг/ч

  • Материал Lithium Battery Materials

  • Продукт Черная месса, Cu, Ал, Сталь

  • Космос Индивидуальный макет

Growing battery retirements are increasing demand for cleaner black mass and higher-value metal recovery. Material liberation directly affects black mass purity and copper foil and aluminum foil quality. Crushing must detach electrode coatings while limiting excessive fines and metal loss. This article examines crushing stages, particle-size control, скрининг, разделение воздушного потока, магнитная сепарация, and commercial performance validation.

How Does a Liberation Circuit Match Black Mass and Metal Product Targets?

01 · Liberation Circuit

Material liberation should follow product specifications, not the smallest achievable particle size. The circuit must release coatings while protecting copper foil, aluminum foil, сталь, и пластик. Поэтому, engineers should define impurity limits before selecting crushers, экраны, and separators. Юшуньсинь reference lines process 500 кг/ч или 1,000 кг/ч. Their listed powers reach 300 кВт и 349 кВт. Both configurations combine physical crushing, разделение воздушного потока, and vibrating screening. They recover black powder, медь, алюминий, и железные фракции.

01

Product Specifications Set Liberation Target

Product Specifications define the Liberation Target for each stream. Черная месса, медь, алюминий, steel and plastic need different purity limits and equipment responses.

02

Controlled Liberation Prevents Value Loss

Controlled Liberation avoids over-crushing and metal loss. Staged crushing, screening and separation improve black mass quality while reducing copper, aluminum and dust contamination.

03

Material Balance Confirms Performance

Material Balance tracks black mass, медь, алюминий, сталь, plastics and losses. Восстановление, purity and recirculation data verify liberation performance after testing.

How Should Feedstock Data Define the Crushing Solution?

02 · Crushing Solution

A crushing line should start with a feedstock map, not a fixed machine list. Формат батареи, химия, charge level, влага, and casing structure change the required pretreatment. Поэтому, two projects with equal capacity may need different shredders, экраны, and safety controls. Yushunxin reference lines cover 500 kg/h at 300 кВт и 1,000 kg/h at 349 кВт. Однако, final power and layout should follow representative material tests.

 

Map the Feedstock Before Selecting the Crusher

Set the Crushing Boundary Through Controlled Pretreatment

Match Primary Shredder Settings to Battery Structure

 

How Does a Staged Liberation Circuit Protect Copper and Aluminum Foils?

03 · Liberation Circuit

Industrial material liberation needs several controlled stages. A single aggressive crusher creates excess fines and lowers metal value. Yushunxin lines combine physical crushing, разделение воздушного потока, и вибрационное просеивание. Reference capacities include 500 кг/ч и 1,000 кг/ч.

01

Primary Shearing
Opens Cells Safely

Primary Shearing opens battery structures while reducing heat and metal powder. Low-speed control helps expose internal layers without excessive foil damage.

03

Secondary Liberation
Releases Electrode Coatings

Secondary Liberation separates electrode coatings from copper and aluminum foil. Proper speed, feed rate and residence time improve black mass quality.

02

Match Equipment
With Liberation Force

Liberation Force should match battery structure and output targets. Измельчение, crushing and milling require different forces to avoid metal pulverization and contamination.

04

Closed Return Loop
Improves Recovery

Closed Return Loop sends unliberated oversize back for further treatment. It reduces over-grinding, protects foils and stabilizes downstream separation.

How Does a Screening Circuit Route Black Mass and Metal Fractions?

04 · Screening Circuit


Screening should control the liberation circuit, rather than simply classify finished materials. Each deck should route fines, metal fractions, and oversized pieces toward different stages. Yushunxin’s reference lines combine crushing, разделение воздушного потока, and vibrating screening. They offer processing capacities of 500 кг/ч и 1,000 кг/ч.

01

Tested Cut Points Build Recovery Route

Tested Cut Points define particle routing and product quality. Material testing helps set screening sizes for black mass, медь, aluminum and plastic recovery.

02

Multi-Deck Screening Stabilizes Separation

Multi-Deck Screening creates stable particle ranges for downstream separation. Different decks reduce interference and improve black mass and metal recovery efficiency.

03

Anti-Blinding Design Protects Material Balance

Anti-Blinding Design prevents blockage from wet powder, films and fine wires. Stable screening improves recovery, reduces re-crushing and protects metal fractions.

How Does a Separation Circuit Route Each Liberated Battery Fraction?

05 · Liberated Battery Fraction

Successful separation starts with material behavior, not with a long equipment list. Engineers should narrow particle sizes before applying magnetic, расход воздуха, гравитация, or electrostatic forces. This sequence protects black mass purity and improves copper and aluminum quality. Yushunxin reference lines combine crushing, разделение воздушного потока, and vibrating screening. Available configurations cover 500 кг/ч и 1,000 кг/ч. Their reference power reaches 300 кВт и 349 кВт.

 

Remove Ferrous Contamination Before Fine Separation

Remove Ferrous Contamination before fine separation. Magnetic drums and suspended magnets reduce iron carryover and protect downstream screening and upgrading equipment.

Use Controlled Airflow For Material Separation

Upgrade Copper And Aluminum Through Gravity Separation

Add Electrostatic Polishing For Higher Purity

Recover Black Mass Through Enclosed Transfer

Match Separation Force With Material Characteristics

 

How Should a Commercial Line Verify Liberation Performance Before Acceptance?

06 · Commercial Line

Commercial acceptance must verify product quality and stable output. Engineers should test the complete line under continuous load. Peak crusher capacity alone cannot prove project performance.

Product Testing Confirms Liberation Quality

Product Testing evaluates Liberation Quality through residual coating, металлическое загрязнение, black mass carryover and ferrous content. These results verify separation performance.

Continuous Operation Proves Rated Capacity

Continuous Operation should verify throughput, product output, recirculation ratio and downtime. Actual capacity depends on battery type and impurity level.

PLC Controls And Feed Trials Confirm Stability

PLC Controls monitor current, температура, кислород, airflow and dust pressure. Feed Trials with different batteries verify stable operation and final product quality.

Краткое содержание

Material liberation determines black mass purity, восстановление металла, and overall line stability. Yushunxin can design a Комплексное решение по переработке литиевых батарей around your battery type, емкость, and product targets. Our scope can cover discharge, сокрушительный, скрининг, разделение воздушного потока, магнитная сепарация, сбор пыли, and PLC control. If you want to get more details for lithium battery recycling, пожалуйста, свяжитесь с нами.

СВЯЗАТЬСЯ С НАМИ

Из ваших потребностей
к реальному воздействию

Индивидуальное решение
ИНДИВИДУАЛЬНОЕ РЕШЕНИЕ
Профессиональная поддержка
ПРОФЕССИОНАЛЬНАЯ ПОДДЕРЖКА
Долгосрочное партнерство
ДОЛГОСРОЧНОЕ ПАРТНЕРСТВО
1 Контактная информация
2 Детали проекта
Форма подписки

Оставьте свое сообщение

Форма подписки
Напишите нам в WhatsApp

Вы не можете скопировать содержимое этой страницы